Purification of metallurgical grade silicon by a solar process

The purification of upgraded metallurgical silicon by extraction of boron and phosphorus was experimentally demonstrated using concentrated solar radiation in the temperature range 1550–1700 °C. The process operated with a flow of Ar at reduced pressure (0.05 atm) for elimination of P, and with a flow of H2O for elimination of B. Impurity content decreased by a factor of 3 after a 50-min solar treatment, yielding Si samples with final average content of 2.1 ppmw B and 3.2 ppmw P.

Download Article

The .pdf version of this article is for internal use only. Do not proceed unless you have the necessary rights.

Proceed Cancel

Reference

G. Flamant, V. Kurtcuoglu, J. Murray, A. Steinfeld. Solar Energy Materials and Solar Cells, 90(14), 2099 - 2106 (2006). doi: 10.1016/j.solmat.2006.02.009